The table below compares European and American Standards for commonly used stainless steel welding filler materials. It is intended to give comparisons only; these may not represent direct equivalents.

BS EN ISO 14343:2007ANSI/AWS A5.9/A5.9M: 2006UNS number
13 ER410 S41080
13 4 ER410NiMo S41086
17 ER430 S43080
19 9 L ER308L S30883
19 9 H ER308H S30880
23 12 L ER309L S30983
23 12 2 L ER309LMo S30986
25 20 ER310 S31080
29 9 ER312 S31380
19 12 3 L ER316L S31683
19 12 3 H ER316H S31680
19 13 4 L ER317L S31783
19 12 3 Nb ER318 S31980
19 9 Nb ER347 S34780
22 9 3 NL ER2209 S39209

Further information

What are the equivalent European and American Standards for common stainless steels?
Welding of austenitic stainless steels - a guide to best practice
Fabrication with low cost stainless steels - a guide to best practice
Arc welding duplex stainless steels - a guide to best practice

For more information please email:


contactus@twi.co.uk