What are the applications of high power electron beam welding?

   

Frequently Asked Questions

Some potential applications of high power electron beam welding are listed below. Many of these are already industrially exploited worldwide

  • Large gas turbines
  • Water turbines
  • Pressure vessels and vacuum vessels
  • Power generation plant
  • Fabrication of large complex products from modular components
  • Defence applications
  • Nuclear waste encapsulation vessels
  • Offshore thick wall tubular components
  • Coal conversion plant
  • Thick section valves, pumps and flange components
  • Large tubular products
  • Repair and reclamation work
  • Composite rolled and forged products
  • Chemical plant

 

High power electron beam welding offers tremendous opportunities for the design and fabrication of thick section components. Here at TWI, we have one of the world's most advanced electron beam welding facilities, backed-up with many year's knowledge and expertise.

Typical weld penetrations with a high power electron beam system.


Power kWMaterialThickness mmWelding speed mm/min
4.5
17
39
53
75
100
low alloy steel
low alloy steel
low alloy steel
low alloy steel
low alloy steel
5083 Al alloy
10
40
85
140
280
270
500
350
150
100
50
600

 