CreepUT An ultrasonic non-destructive testing system for detection and quantification of early-stage subsurface creep damage in the thermal power generation industry.
LaserSnake TWI’s high powered laser cutting technology with an OC Robotics snake-arm robot, giving a decommissioning tool with the dexterity required to work in high-hazard confined nuclear environments.