Who should attend?
All NDT personnel, inspectors and technicians who are involved in in-service inspection, weld inspection or inspection of castings and forgings during fabrication can benefit from this course.
Where can I take the face-to-face training?
The CSWIP Magnetic Particle Testing (MT) course is available in several countries throughout the South East Asia region. You can attend the course in China, Malaysia, Singapore, South Korea and Thailand.
What will I learn?
By the end of the course, you should be able to:
- Explain the basic principles of penetrant inspection methods
- Carry out penetrant inspection using solvent-removable, water-washable and post-emulsifiable/removal processes
- Write clear and concise inspection instructions and test reports
- Meet syllabus requirements for CSWIP Level 2
What are the entry requirements?
There are no mandatory course entry requirements.In order to get certified, you need to successfully complete the examination and obtain the required experience of 4 months for direct entry to level 2.
HRDCorp claimable grant
TWI Training courses are all HRDCorp claimable under the SBL-Khas scheme. SBL-Khas provides opportunity for HRDCorp registered employers to retrain and upgrade their employees in line with their operational and business requirements.
To start your grant application, click here to find out the process flow and guideline.
MBOT Continuing Professional Development (CPD) hours earned
20 hours